MEMSnet Home: MEMS-Talk: tin etchant?
tin etchant?
2003-11-12
Christopher Bailey
tin etchant?
Christopher Bailey
2003-11-12
Hello,

I am wondering if there is any experience with the etching of tin (Sn).
There doesn't seem to be too much information online.  Is there a
commercially available product?  If not, is there a respected mixture of
acids traditionally used for the etching of tin?  Etch rates?

Thanks,
Chris


*************************************************
Christopher Bailey
*************************************************
Office Phone (585) 275-8091
Department of Electrical and Computer Engineering
345 Hopeman Hall
University of Rochester
ROCHESTER, NY 14627
www.ece.rochester.edu/~jones
*************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing