MEMSnet Home: MEMS-Talk: Summary of Electroplating solutions
Summary of Electroplating solutions
1997-02-28
Ken Westra
Summary of Electroplating solutions
Ken Westra
1997-02-28
A number of people ask me to post the results of my quest for various
plating solutions.  Well, here it is:

1) General Info on Plating Solutions

    Electrochemical Sicence and Technology Information Resource
    www.cmt.anl.gov/estir/info.htm
    A very good source of every kind of information on plating you
    would ever want, including the sci.electrochem. FAQ

2) General Plating Suppliers

a) Entone-OMI   has all kindsof plating solutions including permalloy
(the sales guys know it as Nickel-Iron Alloy). They have a web page.
They also have sales offices everywhere.

b) Transene Co
      Rowley MA
     (508) 948 2501
      fax 508 948-2206

c) Plus lots of other smaller companies

The only problem with these suppliers or any other gneral
electroplating solution suppliers is that their smallest container is
a 50 gallon pail.

3) Permalloy

I received a nice paper from Jong-Uk Bu of LG Electronics Research
(Korea). It contains the details on deposting permalloy. His e-mail
address is [email protected]

4) Nickel
    The nickel solutions that people seem to use are the ones that
you can find in any textbook or handbook on electroplating.

Thanks to all the people who e-mailed me  information.

    Ken Westra
    [email protected]
    Alberta Microelectronic Centre


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing