Polyimide vs HF
2004-03-08
li Yu
2004-03-09
C.Y. Hsieh
Polyimide vs HF
C.Y. Hsieh
2004-03-09
The cured polyimide can be removed by oxygen plasma. We do so to use the
testing wafer repeatedly.  But the wafer will become dirty after being
tested for more times.

cyh

----- Original Message -----
From: "li Yu" 
To: 
Sent: Monday, March 08, 2004 11:47 AM
Subject: [mems-talk] Polyimide vs HF


> Dear All:
> I plan to coat Cr and Au on silicon and than put it in conc.HF for 30min,
now I find some problem. now I plan to coat layer of polyimide on Au before
HF as a protecting layer
> 1. the adhension of polyimide to Au is good enough?
> 2. if the polymide is fully cured, can I  get  rid of it by oxygen plasm?
> Thanks in advance!
> Lili
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Yahoo! Search - Find what youre looking for faster.
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.