MEMSnet Home: MEMS-Talk: negative photoresist for ebeam lithagraphy
negative photoresist for ebeam lithagraphy
2004-04-13
LSWANG
negative photoresist for ebeam lithagraphy
LSWANG
2004-04-13
Dear Mems community,
I am looking for a negative photoresit for e-beam
writer. I heard about NEB31 but I can't find where to
buy it. ODea nyone know some other options.
Any informaiton will be appreciated.
Lisen

P.S. Please reply directly to me email address and not
to the entire
MEMS
TALK list.  Thank you.




__________________________________
Do you Yahoo!?
Yahoo! Tax Center - File online by April 15th
http://taxes.yahoo.com/filing.html


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics