Tungsten Etch without etching Silicon
2004-10-04
Menn, Steven
2004-10-04
Kirt Williams
Tungsten Etch without etching Silicon
Menn, Steven
2004-10-04
Dear All,

I am looking for a fairly selective process (5: or better) to strip
patterned Tungsten without etching too much silicon.  Does anyone know
of any dry/wet etch options?  Thank you.

Steve

-------------------------------------------------
Steven Menn, Research Assistant
Boston University Photonics Center
8 Saint Mary's Street
Boston, MA 02215
email: slavam AT bu.edu


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing