2004-10-11
Krishna Vummidi
2004-10-11
PRAMOD GUPTA
2004-10-11
Mark Fuller
2004-10-12
tida
su-8 on glass-edge bead problem
tida
2004-10-12
hi,

you can try the edge beam remover which provided by microchem.

alternatively, you can try the constant volume injection method to
avoid edge beam effect.
http://mml.es.ncku.edu.tw/study/Result/9-page/SU-8_che-hsin.pdf

gd luck n best rgds,
patrick chin



On Mon, 11 Oct 2004 13:41:23 -0400, Krishna Vummidi  wrote:
> Hi,
> Im trying to pattern su-8 on glass (square, rectangular slides). Edge bead
seems to be inevitable. Suggestions on minimizing them would be really
appreciated. thanks, krishna
>
> ``````````````````````````````````````````````````````````````````````````````
```````````````````````````````````````````````````
> Krishna Vummidi
>
> GRA, Wireless Microsystems Lab (www.ece.vt.edu/wml)
> The Bradley Department of Electrical and Computer Engineering
> Virginia Polytechnic Institute and State University
> 433 Whittemore Hall (Mail Code 0111), Blacksburg, VA 24061
>
> (540) 231-3411 (Voice) -3362 (Fax)        E-mail: [email protected]
>
> ``````````````````````````````````````````````````````````````````````````````
```````````````````````````````````````````````````
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation