Are you sure?
I look for another paper and get the Young's modulus of TaN is
150GPa~250GPa!
So I don't know which one is correct.
Anyone can tell me what value is correct?
----- Original Message -----
From: "Suhua Jiang" 
To: 
Sent: Friday, October 15, 2004 12:23 PM
Subject: RE: [mems-talk] TaN


> 455GPa
>
> >From: 童麒嘉 
> >Reply-To: General MEMS discussion 
> >To: 
> >Subject: [mems-talk] TaN
> >Date: Tue, 12 Oct 2004 19:36:07 +0800
> >
> >Dear all,
> >             Anyone can tell me the Young's modulus of Tantalum nitride?
> >             Or any textbook can find this data?
> >          Thanks
> >           Rasheed
> >_______________________________________________
> >[email protected] mailing list: to unsubscribe or change your list
> >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> >Hosted by the MEMS Exchange, providers of MEMS processing services.
> >Visit us at http://www.memsnet.org/
>
>
> National Microanalysis Center
> Materials Science Department
> Fudan University
> 220# Handan Road
> Shanghai, 200433
> China
> Tel: 86-21-65642380
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing