MEMSnet Home: MEMS-Talk: RE: Spam:[mems-talk] how to spincoat a 50nm thin uniform film of AZ9260?
RE: Spam:[mems-talk] how to spincoat a 50nm thin uniform film of AZ9260?
2004-10-19
Z. Jiang
RE: Spam:[mems-talk] how to spincoat a 50nm thin uniform film of AZ9260?
Z. Jiang
2004-10-19


hi Matthew,

   Thanks for you information. The black 'beads' I observed in the thin
filmm are a few microns diameter and as the dilution ratio enhances from
1:5 to 1:50, their number reduces. I think probably submicron filtration
will work. What commercial company do you know that provides good filters?

   Could you please explain what "heating under reflux" method means, and
how to spin at temperature? Our spin-coater doesn't have a heater with it.

  Cheers

  Jiang



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.