MEMSnet Home: MEMS-Talk: RE: thermal or optical releasable polymer
RE: thermal or optical releasable polymer
2004-11-17
WALTER Harald
2004-11-17
[email protected]
2004-11-18
Chris Folk
RE: thermal or optical releasable polymer
WALTER Harald
2004-11-17
Dear Gene,

Edward De Meter of Penn-State-University (http://www.psu.edu/) published
a glue which hardens by illumination with UV and gets brittle under IR.
I don't know if the glue is applicable to your wafers.

Harald



> I am looking for polymer that can joint two wafers (Si-to-Si or
> Si-to-glass) temporarily for processing, and then can be separated
> (released) by either thermal or optical (UV) treatment.
> Anyone has the vendor info, please let me know. Thanks!
> Gene
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing