A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Quick Test of Silicon orientation
Quick Test of Silicon orientation
2005-05-10
Christoph Wild
2005-05-10
Kenneth Smith
2005-05-12
Roger Brennan
Quick Test of Silicon orientation
Roger Brennan
2005-05-12
If the wafers are not polished on both sides, look at the rough side under a
microscope.  You will usually see rectangles and squares if it is <100> and
equilateral triangles if it is <111>.

Roger Brennan

-----Original Message-----
From: Christoph Wild
Subject: [mems-talk] Quick Test of Silicon orientation

I have ordered a batch of silicon wafers without flat.
We ordered 100 oriented wafers, however, now it turns out that some of the
wafes are 111 oriented.
Is there a quick test which allows us to discriminate between 100 and 111
oriented wafers ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering