A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Wet-Etch SiO2/Si3N4
Wet-Etch SiO2/Si3N4
2005-05-12
Josef Kouba
2005-05-12
[email protected]
2005-05-12
Brent Garber
2005-05-12
[email protected]
Wet-Etch SiO2/Si3N4
[email protected]
2005-05-12
BHF/BOE

-----Original Message-----
From: Josef Kouba 
Subject: [mems-talk] Wet-Etch SiO2/Si3N4

what is a good wet etchant for SiO2 which leaves Si3N4 intact?