I'm not sure about HF but acetone does not attack Cu.

Tony Galindo

-----Original Message-----
From: Tan, Chuan Seng 
Subject: [mems-talk] HF and Cu

Can anyone tell me if diluted HF (say 1:20) attacks Cu ? And does Acetone do
anything to Cu ?