how to pattern frit glass on si wafers
2005-05-17
NL
2005-05-17
Eric Miller
how to pattern frit glass on si wafers
Eric Miller
2005-05-17
Nielei,

Typically, glass frit is screen printed.  We have a system and process set
up that works fairly well.  Feel free to contact us if you have any specific
questions.

Eric Miller
WTC Microfab Lab
206 616-3855

-----Original Message-----
From: NL
Subject: [mems-talk] how to pattern frit glass on si wafers

Dear all:
    Now I`m looking for a meathod to pattern frit glass  on Si wafers.
The frit glass is gel-like.So I can`t do it by lift-off.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review