A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: residues on RIE etched sio2
residues on RIE etched sio2
2005-05-23
yilei zhang
2005-05-23
[email protected]
2005-05-24
yilei zhang
2005-05-24
Paolo Tassini
2005-05-25
yilei zhang
2005-05-25
Isaac Wing Tak Chan
residues on RIE etched sio2
[email protected]
2005-05-23
Yilei:

You can first use 100% oxygen plasma to remove polymer then follow with
H2SO4+H2O2 wet bath at 100 degrees C rinse with di water then place in HF
solution for removal of SIO2 remaining mask. Bob Henderson

-----Original Message-----
From: yilei zhang 
Subject: [mems-talk] residues on RIE etched sio2

Hello colleagues:
I used rie (10% O2, 90% CF4) to etch silicon with a polymer layer and a sio2
mask, but found the left sio2 cannot be further etched away with HF. I
searched the archive and found the RIE may generate a polymer layer or
fluorocarbon, and a layer of fluorinated si. I want to know is there any way
to remove the left sio2 mask? Thanks.

Regards,
Yilei Zhang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
University Wafer