si etch help
[email protected]
2005-05-27
The cause might be the temperature.  how hot is the wafer getting?

-----Original Message-----
From: babitha bommalakunta 
Subject: [mems-talk] si etch help

I am trying to work out Si etch process with CF4 and O2 combination in pecvd
system.My sample appears white after etching . Any idea due to what this
happens?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics