A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Gold etching
Gold etching
2005-11-30
Sebastien Allard
2005-12-01
Zhang Peng
2005-12-01
Shay Kaplan
2005-12-01
Michael D Martin
2005-12-02
Sebastien Allard
2005-12-02
Bill Moffat
2005-12-02
Sebastien Allard
2005-12-02
David Nemeth
2005-12-05
Manish Hooda
2005-12-02
[email protected]
Gold etching
David Nemeth
2005-12-02
See http://www.mems-exchange.org/catalog/lift_off/

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA 20151


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Sebastien Allard
Sent: Friday, December 02, 2005 10:59 AM
To: General MEMS discussion
Subject: [mems-talk] Gold etching


Unfortunately, I am not familiar with lift-off?  Is this a process or a
product?

Thanks!

Sébastien Allard
LxSix Photonics
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.