A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: hot plate recommendation
hot plate recommendation
2006-01-06
[email protected]
2006-01-07
Neal Ricks
PMMA solution
2006-01-09
Jure Simcic
2006-01-09
Hongjun-ECE
2006-01-10
Sebastien Allard
hot plate or infrared?
2006-01-10
Andrew Xiang
vacuum baking?
2006-01-10
Andrew Xiang
Wet etching? Dry etching?
2006-01-10
sokwon Paik
2006-01-11
Hongjun-ECE
2006-01-16
Aegis Liang
2006-01-10
Novak Farrington
hot plate recommendation
[email protected]
2006-01-06
Hello all,

I'm looking to purchase a programmable hot plate for our lab to do baking of
photoresists for photolithography. I'm looking for one where I can control the
ramp of heating and cooling (i.e. tell it to increase its temperature at 2
C/min then stay at some temp for a while and then cool at 1 C/min). If anyone
could recommend a brand or model to me I would greatly appreciate it.

thanks,
Joe Grogan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing