MEMSnet Home: MEMS-Talk: Ohmic contact to Silicon
Ohmic contact to Silicon
2006-02-02
Kamesh
2006-03-07
Roger Brennan
Ohmic contact to Silicon
Kamesh
2006-02-02
Hi All,

I am fabricating a P+Si/P GaAs heterojunction diode. I have read that
Ti/Al can be used to make an ohmic contact to Silicon. Can anyone
please advise the thickness of Ti and Al and the time/temperature of
anneal ? Is the anneal to be carried out in an RTA oven ?

Thanks you.
Regards
Kamesh