A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE : [mems-talk] Encapsulant for wire bonding
Encapsulant for wire bonding
2006-02-09
FrançoisTherriault Proulx
2006-02-10
Jesse D Fowler
RE : [mems-talk] Encapsulant for wire bonding
2006-02-10
Sebastien Allard
2006-02-09
Sebastien Allard
Is chromium mask is chromium oxide or chromium?
2006-02-10
sokwon Paik
Is chromium mask chromium or chromium oxide or both?
2006-02-10
sokwon Paik
2006-02-10
[email protected]
RE : [mems-talk] Encapsulant for wire bonding
Sebastien Allard
2006-02-10
Nail polish?  Interesting application  I used to stuff to mask gold from =
TFA gold etch.  The problem is, you can't really buy the stuff in big =
quantities - one way is to buy "lacquer" (Minwax or other brand as long =
as it is lacquer) at your hardware store.  You can dilute it with =
acetone to get the viscosity you want.  Acetone is also the way to go to =
remove it.
=20
S=E9bastien Allard
R&d Process Engineer
LxSix Photonics

________________________________

De: Jesse D Fowler
Date: jeu. 2006-02-09 19:10
=C0: [email protected]; General MEMS discussion
Objet : Re: [mems-talk] Encapsulant for wire bonding

Hi Frank,

Would you believe...

Nail polish?

Some associates of mine are using it to insulate gold wire bond wires =
from
mercury. They say most types work, except "glitter" nail polish.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange