MEMSnet Home: MEMS-Talk: Transparent POlymer or adhesive for quartz
Transparent POlymer or adhesive for quartz
2006-03-14
Aashish Singh
2006-03-14
Matthew Coda
Transparent POlymer or adhesive for quartz
Aashish Singh
2006-03-14
  Dear All,

  I'm looking for a Transparent Polymer/Adhesive with very large dn/dT, that can
be spin coated over quartz. i have tried popular Norland Optical adhesive, but
its dn/dT is not as large as i want. The polymer/adhesive we will use at both
visible and IR region. The dispersion curve (variation of R.I with Wavelength) ,
dn/dT and  low absorption at the wavelength of operation is important for my
applications.
  Any information and the source form where we can get it will be highly
appreciated.
   Thanks in advance.
Aashish singh
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation