How to analyse surface conditions?
2006-04-27
Wullinger, Michaela
2006-05-01
Kirt Williams
How to analyse surface conditions?
Kirt Williams
2006-05-01
Measuring the contact angle of a drop of water will give you an idea of
whether you have clean glass (the water spreads)
or you have an organic coating (the water beads up).
    --Kirt Williams

----- Original Message -----
From: "Wullinger, Michaela" 
To: 
Sent: Thursday, April 27, 2006 12:05 AM
Subject: [mems-talk] How to analyse surface conditions?



Hi
I'm looking appropriate methods to analyse the surface conditions during
processing  of masks.
What I need to know: contaminations? Surface bonds? H2O content?

Which methods can you suggest?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing