MEMSnet Home: MEMS-Talk: Electroless Nickel Plating
Electroless Nickel Plating
2006-05-08
ravi deverkadra
2006-05-09
Zhang Xiao Qiang
2006-05-09
g.balsubra manian
Electroless Nickel Plating
Zhang Xiao Qiang
2006-05-09
Why do not you try electroplating? It will e selective.

Thank you & have a nice day!
Best regards!

XiaoQiang




-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of ravi deverkadra
To: [email protected]
Subject: [mems-talk] Electroless Nickel Plating

Hello everyone,

I am trying to do some electroless nickel plating using Technic Inc,
solutions. I am having a problem in patterning this nickel, I tried to use a
sacrificial photoresist but the electroless nickel plating is not very
selective its plating everywhere. Any suggestions on this?

Ravi
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing