A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: stress induced by backgrinding
stress induced by backgrinding
2006-05-23
[email protected]
2006-05-23
Martin J Prest
2006-05-23
Tom Bristow
stress induced by backgrinding
Martin J Prest
2006-05-23
Is it tensile or compressive stress? What are typical values of bow?
Are wafers likely to break during hard or vacuum contact in a mask aligner?

Martin.