Hello all,

recently I work with SU-8 2100, I have problem with not smooth surface on the
side wall ( I used emulsion film mask).  could any body give me some suggestion
to solve my problem , and also how to increase adhesion between glass and su-8.

thank you very much

regard

sugeng
Yeungnam University, South korea
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation