MEMSnet Home: MEMS-Talk: Planar deposition of PI 2610
Planar deposition of PI 2610
2006-06-30
kris
2006-06-30
Rajib Ahmed
2006-06-30
Bill Moffat
2006-06-30
PRAMOD GUPTA
Planar deposition of PI 2610
Bill Moffat
2006-06-30
Spray.  Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of kris
Sent: Thursday, June 29, 2006 5:21 PM
To: [email protected]
Subject: [mems-talk] Planar deposition of PI 2610

Hello All,

I am trying to deposit(spin) polyimide PI 2610 on the substrate that has
features ranging from 1 to 5um in depth. I am spinning PI2610 for the
planar deposition on the top of the etched features. I need 1um thick
ployimide.

After spinning the PI at 4000 r.p.m. for 30 seconds, i can see the PI
deposition as a conformal deposition rather than the planar deposition.
I can see that the etched pits were covered only by 1um Polyimide. I
want the features to be filled up completely. I dont want any crests or
troughs on the sample when i scan the profilometer over the features.

In short, can someone suggest me the procedure to get the planar
deposition of the PI2610 on the substrate that has different depth
features.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing