Dicing Tape
walter essinger
2006-08-07
I am curious can you share the dimension of the smallest holes.
Are they less tha 50-75 mirons.,we have problems making them
Thanks
Walter
----- Original Message -----
From: "Mac McReynolds" 
To: 
Sent: Friday, August 04, 2006 8:01 AM
Subject: [mems-talk] Dicing Tape

> I'm going to be running some trials with highly polished glass substrates
> full of through holes.  I find many vendors who offer "High Tack" UV
> dicing tape, but they all seem to use different units and methods of
> characterizing adhesion.  Can anyone in the group save me the trouble of
> running a test matrix and recommend the highest tack tape from practical
> experience.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.