MEMSnet Home: MEMS-Talk: Resist Recovery Method
Resist Recovery Method
2006-08-07
Ron Martin
2006-08-08
Bill Moffat
Resist Recovery Method
Bill Moffat
2006-08-08
Ron,
    In a previous life I worked for a small chemical company called
RhoChem.  They tried to sell reconstituted resist.  They would filter,
clean and prepare the resist using Gel Permeation Chromatography to
demonstrate the recovered resist was identical to the original at half
the price.  The total interest at just about all the major resist users
was zero.

Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Ron Martin
Sent: Monday, August 07, 2006 4:13 PM
To: 'General MEMS discussion'
Subject: [mems-talk] Resist Recovery Method

Has anyone tried to recover used resist?  If so, what is your filtration
and reconstitution method?  Do you check viscosity?  How about third
parties interested in buying used chemicals?  I appreciate your input.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing