I am  trying to deposit Ag or Pt as electrodes on the soda lime glass
slide. The evaporator environment is not that clean as it is not in my
own lab. Could someone tell me the effect of impurity on the metal
deposition. If the impurity gets deposited along with the metal then
how is it going to effect my deposition as well as my readings.

--
RUPESH SAWANT
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.