MEMSnet Home: MEMS-Talk: 10 nanometer hole
10 nanometer hole
2006-08-17
[email protected]
2006-08-17
Roger Shile
2006-08-18
Isaac Chan
2006-08-19
Jacques Jonsmann
2006-08-20
Jeehwan Kim
2006-08-22
Glenn Silveira
2006-08-21
Glenn Silveira
Re: 10 nanometer hole
2006-08-18
mohendra roy
2006-08-21
Jim Beall
2006-08-19
[email protected]
2006-08-21
[email protected]
2006-08-21
Rob Knobel
2006-08-21
[email protected]
10 nanometer hole
Roger Shile
2006-08-17
Drill 1/5 of the way through:)

-----Original Message-----
Does anyone know how and who can make a 10 nanometer hole in a 50 nanometer

film.

Thank you.

John  Bishop
President
Norsam Technologies,  Inc.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.