MEMSnet Home: MEMS-Talk: Re: Problems with my Ti/Au wet etching process
Re: Problems with my Ti/Au wet etching process
2006-09-26
Vinay
2006-09-26
[email protected]
2006-09-27
Brad Cantos
2006-09-28
deepa sree
2006-09-27
Vinay
2006-09-27
Roger Shile
Re: Problems with my Ti/Au wet etching process
Brad Cantos
2006-09-27
Yes, this is a very strong GaAs etchant.
Brad

On 9/26/06 7:02 AM, "[email protected]"  wrote:

> Vinay,
> Does this etch etch thourgh GaAs or AlGaAs?
> Ali
>
>
> Quoting Vinay :
>
>> Hi Ali,
>> One possible recipe to etch Ti is:
>> 20H2O(DI) : 1HF : 1H2O2.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation