Polymerisation of PDMS
Barbara Cortese
2006-10-03
Hi

try using an oven with 140°C for 15 minutes!


---------- Initial Header -----------


> Subject : [mems-talk] Polymerisation of PDMS

> Hello everybody,
>
> Please, someone can tell me which is the  temperature and time for complete
> polymerisation of PDMS ? I know there is many process on it but in your
> opinion which is the best ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing