MEMSnet Home: MEMS-Talk: Nickel nanodots annealing!!
Nickel nanodots annealing!!
2006-10-04
madhav rao
how to pattern PDMS film
2006-10-05
Jianhua Tong
Nickel nanodots annealing!!
madhav rao
2006-10-04
Hi everyone,
            I am having doubt on whether we can anneal
Nickel nanodots at around 300-500 degree celcius,
after depositing nickel nanodots. I am looking forward
to deposit nanodots & then anneal it, since  this
gives me selective growth of nickel nanodots rather
than going for nickel thin film & using nucleation -
annealing process. Under what conditions i can anneal
nanodots like whether i need to go for nitrogen gas or
some other ambient.

Please let me know about this as soon as possible

Thanks


Regards,
Madhav
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review