A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Partial Metallization of Vertical Walls
Partial Metallization of Vertical Walls
2006-10-13
Xiaoguang "Leo" Liu
2006-10-14
Florian Herrault
2006-10-16
Beggans Michael H IHMD
2006-10-16
Xiaoguang "Leo" Liu
Partial Metallization of Vertical Walls
Xiaoguang "Leo" Liu
2006-10-13
Dear all
I've been working on a project in fabricating cavity electromagnetic
resonators that require partial metallization of the side walls. For
example, I would like to produce a rectangular cavity  in the silicon
substrate by DRIE. I would then want 2 of the 4 side walls to be
metallized with gold while keeping the other 2 silicon. I've thought
really hard about this but could not find a way to meet the
requirement. The cavity in consideration is about 1mmx1mm big.

Does anybody have good suggestions? Thanks a lot

Best
Leo

--
Xiaoguang "Leo" Liu
Electrical and Computer Engineering
Purdue University
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing