Nickel electroless Plating!!
David Roberts
2006-11-03
Hi Madhav,
Is the PMMA breaking down due to the high temp. E-less process?  One
approach would be to initiate the deposition at high temp. and then move the
part into a lower temp solution say 50 C. What about electrolytic
deposition?
Regards,
Dave

-----Original Message-----
From: madhav rao [mailto:[email protected]]
Sent: Thursday, November 02, 2006 4:48 PM
To: General MEMS discussion
Subject: [mems-talk] Nickel electroless Plating!!

Hi All,
        I am not able to find a simple way of doing
electroless Nickel plating on PMMA patterned silicon
wafer. Can any one provide me any PDF file or any
procedure to do Electroless Nickel plating.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review