MEMSnet Home: MEMS-Talk: How to clean single crystal TiO2 with chemicals?
to get thin SU-8 film
2006-10-29
[email protected]
2006-11-01
Gareth Jenkins
Flow sensor inquiry
2006-11-01
Rajib Ahmed
How to clean single crystal TiO2 with chemicals?
2006-11-01
Xiaojing Zou
2006-11-04
VS Bhat
How to clean single crystal TiO2 with chemicals?
VS Bhat
2006-11-04
Dear Mr.Xiaojing,
H2O2 and HF or HNO3 and HF mixtures are generally used for Ti etching. May be
one of them can be tried if their use is not a problem in you case
Bhat
Quoting Xiaojing Zou :

> Hi:
>
>     Is there anybody having experience with wet etching single crystal TiO2
> substrate??? I want to etch the surface for half micron deep.  I tried H2SO4
> and HF, but it does not do the job. But as far as I know, acid will attach
> TiO2.
>
>    I do not quite understand why it is so hard to etch single crystal
> materials??
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing