Re: Trying to Study Diffusion profile
abdelyamine
2006-12-02
To do good profile of diffusion you need to do an ionique implantation.

Summary of Ion Implantation:



          Dope semiconductor

          Better doping method than diffusion

          Easy to control junction depth (by ion energy) and dopant
concentration ( by ion current and implantation time).

          Anisotropic dopant profile.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics