Hi,
we are a small startup in France and we are trying to do a backside
plasma etch with an aspect ratio of 1:10 on 200 mm silicon wafers. We
also need to align these trenches with patterns on the front side of the
wafer.  I woudl appreciate if you could point us to some foundries that
would take up this lithography and etching process. Can you also give me
a cost estimate on this process.
thanks
prashanth
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing