Wet etching thickness technique with smooth surface
2008-08-16
Moshe
2008-08-17
Andrea Mazzolari
2008-08-19
P.E.M. Kuijpers
2008-08-19
Moshe
Wet etching thickness technique with smooth surface
P.E.M. Kuijpers
2008-08-19
Hi,

Is this only for getting a thinner Si wafer?
Then you can also perform grinding or ultrafine grinding followed by CMP
..

Peter Kuijpers
mailto:[email protected]


---- Original Message ----
From  Moshe   
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.