Hi all,

Does anyone have experiences on using Ebeam evaporator to deposit TiO2 thin
film? In our system, the pressure is very high when TiO2 is heated, and crystal
monitor cannot read the rate very stably. Could anyone give some suggestions?

Thank you.

------------------
Best regards,

Xing Sheng

2013-04-10
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing