MEMSnet Home: MEMS-Talk: micron size holes in SU8
micron size holes in SU8
2013-06-04
Antoine Blin
micron size holes in SU8
Antoine Blin
2013-06-04
Hi,

I am searching to make 2 - 5 microns diameter holes in SU8 within a 20 -
40 microns thickness range, of course with a chrome mask.
Anyone would have a good recipee (exposure seems very important,
cycles?, filters?..)?

Regards,

Antoine
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics