Hi All,

I was wondering why does Copper susbtrates require higher exposure dose. I
understand that it has something to do with the reflection from the copper
substrate. Can anyone explain it.

Many Thanks,
Ricky Anthony
Tyndall National Institute
Cork, Ireland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing