Hi,

I am currently doing electrostatic MEMS device and have to deal with
PFDA coated on ALD Alumina. But seems the stiction and adhesion are
still large. I wonder if anyone of you have done surface treatment
before the deposition of PFDA on alumina? Thanks.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group
University Wafer