2014-01-07
DEBASHIS MAJI
2014-01-07
André Bödecker
2014-01-07
Jan Thoren
2014-01-08
DEBASHIS MAJI
2014-01-08
DEBASHIS MAJI
2014-01-09
Jan Thoren
2014-01-09
James Guenes
2014-01-09
DEBASHIS MAJI
2014-01-10
André Bödecker
2014-01-09
Jan Thoren
2014-01-08
James Guenes
2014-01-08
王舒禹
Bio-compatible epoxy
Jan Thoren
2014-01-07
I have a material which is friendly to the human body and has very good
bonding abilities . It is non - conductive.
What is the substrate material?
I would be willing to test it if you can provide a sample of the material.
My email is [email protected]




Recreating Architecture through Nanotechnology


JanThoren-president
NanoArchitech
Architectural Technology Group
San Francisco Bay Area

707 741-7919 direct line

nanoarchitech.com







On Sun, Jan 5, 2014 at 10:27 PM, DEBASHIS MAJI wrote:

> Dear All,
>
> I am searching for a some biocompatible epoxy (not conductive epoxy) to fix
> my sensor over a substrate for some in vitro animal experiments. can
> anybody kindly provide me names of few such epoxies?
>
> Thanks in advance.
>
> --
> Thanks & Regards
>
> Debashis Maji,
> Senior Research Fellow,
> PhD Scholar - School of Medical Science & Technology,
> IIT Kharagpur, India - 721302
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group