SU8 aspect ratio
João Tiago dos Santos Fernandes
2014-05-06
Can't you achieve those specification by using SU-8 50 and the protocol
suggested in the datasheet?

- João Tiago
________________________________
From: bhargav panchal
Sent: ‎06/‎05/‎2014 18:34
To: General MEMS discussion
Subject: Re: [mems-talk] SU8 aspect ratio

Hi



You can go for the BOSCH DRIE process....  provides very high aspect ratio...
not sure...consult...and let me know...




On Tuesday, 6 May 2014 9:23 PM, Antoine Blin  wrote:

Hi everyone,

I am using standard techniques for fabricating SU8 mould for
microfluidic PDMS devices, but i am having troubles obtaining a correct
aspect ratio.

  Does anyone have some tips to achieve a:
- 50 µm height
- 10 µm width pattern
- a 0 - 3 µm variation in width of the pattern between substrate and the
top.

The resolution of the mask (SELBA, Switzerland) is checked and good, I
am working in hard contact, and use a 365 nm i-line filter for the exposure.
I may think this is related to diffraction, would you suggest to use:
- under exposure?
- flash exposure?
- other ideas??

I also tried multi layers to minimize the diffraction effect on each
step, but the pattern is particulary difficult to align (big area and
small parallel patterns..)

Thank you for your help!

Antoine Blin

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group
Harrick Plasma, Inc.