RIE Silicon etching
2014-07-23
Sebastian R Freeman
2014-07-24
Deep Mukhopadhyay
2014-07-25
Lijun Yan
2014-07-24
Sophie Roman
2014-07-25
James Guenes
2014-07-24
Andrew Sarangan
2014-07-25
Sergey Afanasyev
2014-07-25
Ang, Jun'An - angjy006
RIE Silicon etching
Sophie Roman
2014-07-24
Hi Sebastian,
I've seen similar problem with RIE and I think you can try to glue your
wafer, to prevent it overheating.

Best,

Sophie


Postdoc, Stanford University
Energy Resources Engineering Department





2014-07-23 8:00 GMT-07:00 Sebastian R Freeman :

> Hi everyone,
>
> I am etching a 4-inch silicon wafer in the RIE using O2, and CF4, in
> combination. Using positive photoresist, my goal is to create an array of
> silicon pillars covering the surface of the wafer. I am trying to push the
> limits of the machine, and trying to etch several microns. I etched for 5
> minutes and was able to get 1.5 micron tall pillars, the wafer came out of
> the machine very dirty, with a film-like residue on it, and looking very
> scratched up. I think I might have an idea of what this is, but I would
> appreciate anyone else's input, or a way to prevent it.
>
> *Sebastian Freeman*
> *Ph.D Student*
>
> *Binghamton University *
>
> *Thomas J. Watson School of Engineering*
> *Department of Bioengineering*
> *Office: Biotechnology Building 2629*
> *E-mail: [email protected] *
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing