Mr. Yobas,

Supercritical desiccator I have found and used is a small equipment made in
UK, which have a high-pressure chamber, a steel container for liquid CO2 and
a temperature monitor.

I think any supercritical desiccator is ok; however, a small-chamber dryer
means a short release time as well as less CO2 exhaustion.

Good fortune,

Liuqiang Zhang


-----Original Message-----
·¢¼þÈË: Levent Yobas 
ÊÕ¼þÈË: [email protected] 
ÈÕÆÚ: 1999Äê4ÔÂ27ÈÕ 3:33
Ö÷Ìâ: supercritical desiccator


>
>Mr. Zhang,
>
>I have just seen your following mail. I am facing a similar stiction
>problem and planning to get a supercritical desiccator. I will be very
>appreciate if you can share with me valuable replies you got.
>
>sincerely,
>Levent Yobas
>Case Western Reserve University,
>Cleveland OH
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer