MEMSnet Home: MEMS-Talk: RE: Anodic Bonding
RE: Anodic Bonding
2000-03-28
Lapp, Daniel S
2000-03-29
Mirza Andy
2000-03-31
Heeren, Henne van
RE: Anodic Bonding
Mirza Andy
2000-03-29
Dear Sandra Bermejo Broto,

EV Group has the EV500 series of bonders which can be used for anodic,
thermocompression and silicon direct bonding in one system. Our design and
manufacturing center in Schaerding, Austria (+43 7712 53 11-0) can help you
with any custom requirements for your bond process.
EV Group and its high-volume production partners have produced tens of
millions of anodically bonded MEMS devices on the EV500 series of bonders. I
would refer to the article published in SENSORS on this matter by Electronic
Visions and MIT - A.R. Mirza and A.A.  Ayon, SENSORS, December 1998, Vol 15,
No 12, p24-33.
Please e-mail  [email protected]    for copy of this
review paper on silicon wafer bonding.

Best Regards,

Andy Mirza
Technology Manager

EV Group-Technology, Tel: (602) 437 9492 x 112, Fax: (602) 437 9435
E-mail: [email protected]   , Web:
www.EVGroup.com  , Date: 3/29/2000
==============================================================
                -----Original Message-----
                From:   [email protected] [mailto:[email protected]]
                Sent:   Friday, March 17, 2000 6:38 AM
                To:     [email protected]
                Subject:        Anodic Bonding

                Hello,
                I am working in silicon anodic bonding and I would like to
have information
                about this technique. I need the name of companies dealing
this field,
                since I want to buy the tools to implement it.
                Thanks in advance,
                Sandra

                *********************************************************
                Sandra Bermejo Broto
                Semiconductor Devices Group (GDS)
                Electronic Engineering Department
                UPC-Campus Nord, C5
                Jordi Girona, 1-3
                E-08034 Barcelona
                SPAIN
                Phone: + 34 93 401 74 81
                Fax:       + 34 93 401 67 56
                e-mail: [email protected]
                *********************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer
Addison Engineering