A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Negative Photoresist
Negative Photoresist
2002-01-29
Peng Jin
2002-01-29
Paolo Bondavalli
2002-01-29
Matthieu Guirardel
2002-01-29
Michael Yakimov
2002-01-30
Perroud, Olivier
Negative Photoresist
Paolo Bondavalli
2002-01-29
Hi Peng,
The best is BCB by DowCorning.
I also know PDMS by Wackerchemie or Gelest but it's quite difficult to
obtain.
Bye

Peng Jin a icrit :

> Hi, friends,
>
> In my research project, I need to find a kind of negative photoresist which
> must be easy to remove by acetone or other chemical solvent. Could anyone
give
> me some idea about it?
>
> Thanks.
>
> Peng Jin
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

--
*********************************************************
Dr. Paolo Bondavalli
R&D Engineer
LABCOM - Laboratoire Interconnexions Optiques et MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************************
Disclaimer: Opinions expressed herein are my own and may
  not represent those of my employer.
**********************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics