Anodic Bonding of Ferrous alloys to Pyrex
[email protected]
2002-04-03
Has anyone of you tried to bond anodically Pyrex (or another glass) to Ferrous
alloys (Fe-Ni-Co or Fe-Ni) ?  I was told that it was possible with a prior
oxidation of the alloy.  Do you think it's true ?  Do you have practical
information about the preoxidation treatment that is needed ?     Do you think
that a good surface state (roughness etc...) can easily be obtained with ferrous
alloys ?

Thank you in advance !

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing