removing dies from packages
Andrew Cao
2002-04-09
Hi
I'm trying to remove the dies from a TO-92 pacakge.
Does anyone know of a chemical that can dissove the
plastic package without damaging the die.  Would a
oxyen plasma be able to burn off the plastic.  Thanks
Yahoo! Tax Center - online filing with TurboTax
http://taxes.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer